TOP: With perforated materials especially, flatness deviations and high internal stress are a regular occurrence. Leveling perforated parts and sheets is an absolute must to achieve a high-quality final product. BOTTOM: Running a laser-cut part through a part leveler will remove stresses and render the part flat. It’s important to maintain flatness to enable downstream processes to be done accurately and efficiently.
How many times have you fabricated a part that didn’t quite form correctly, bend well, or couldn’t be welded properly?
You might have drilled countersink holes and beveled edges. You put work and time into the part, and now you’re forced to just throw it in the scrap bin and wait for next week when it’s hauled to the scrapyard, netting nickels on the pound.
It’s possible for you to dodge the scrap bin by using a part leveler.
Leveling a laser-cut, plasma-cut, or stamped part might not strike you as being a necessity. For downstream processes, however, a leveled part means a better fit in final assembly. And that’s just the beginning.
What Is Leveling? How Is it Different From Straightening?
Many deformities and stresses in the raw material occur during the initial steel production in the mills. Flatness deformities include edge waves, center buckles, and crossbow. Furthermore, the internal stresses cause springback and warping. The coil tends to retain the natural curvature that the coiling process produces.
To release those trapped internal stresses, you need to bend the material close to or past the material’s yield point.
Stress Relief. Anything that has to be welded or assembled should be flat so that it fits precisely without gaps and bows. However, the minute you start cutting and welding, you’re introducing heat into a part, so it’s going to tend to warp. If it doesn’t warp, it will have high internal stresses. Those internal stresses in the material become apparent in the form of springback and bowing, which make it very difficult to achieve a consistent cutting or welding result.
A part and coil leveler removes those deformities by bending the material close to or past its yield point and then bending it back into a flat state. That is the only way to remove up to 99% of the residual stresses. If you don’t bend it strongly, you will not release that tension or stress.
The yield point varies depending on how severe the deformities are, how many cutouts the part has, and other material specifications.
A rough rule of thumb is that the first set of rollers on a leveler are set at less than the actual material thickness, usually between 40% and 70%. The last set of rollers are always set close to the actual material thickness.
A leveler can have up to 21 rollers. As the material (shown in red) goes through the series of rollers, stresses are removed and the desired flatness is achieved. The rollers underneath the main leveling rollers are backups for maximum rigidity and machine longevity.
For example, a leveler that has 21 rollers will have 10 at the top and 11 at the bottom. There is a gap between the first set of rollers where the material enters the leveler. It is usually set to less than the actual material thickness, so that when the material goes in, it is bent very severely. Then, as the material exits past the last set of leveling rollers, it is flat and stress relieved. The leveling process does not alter the physical size or internal structure of the material.
Leveler, Straightener. A misunderstanding persists regarding straighteners and levelers. A straightener might be a three- or four-roll bender. Often, it takes a skilled operator to turn the part around and put it in again to make the part flat. But that does not remove any of the residual stresses. The problem with a simple straightener is that although you can get the part to lay somewhat flat, you’re just pushing the internal stresses around and not removing them.
Even though the parts look straight and flat, they warp the minute they are heated during fabrication. The parts still have high internal stresses because they were not leveled close to or past their yield point. When they reach the welder, who tries to weld six parts together, they’ll clamp all the parts in place. But guess what will happen during welding? The parts start to bow and the welds are not accurate.
Eliminate Rework. Leveling parts saves fabricators from rework because fabricating flat and stress-relieved parts can then go right to the next fabrication process. They should be perfectly flat to be welded together in an assembly.
What Are the Capacity Limits of a Leveler?
In terms of machine power, there usually are no limits. However, you can be limited by sheet and part size as well as thickness. If you can bend it, you can level it, for the most part. These precision levelers are extremely robust and powerful. They can handle anything from soft alloys like copper, all the way up to ballistic armor AR-500 material for tanks.
Material Thickness, Width. Most coils are about ½ in. thick to 72 in. wide. Coil levelers can level that range.
For plate-thick blanks, a stand-alone leveler can handle up to 2½-in.-thick plate.
Floor Space. Obviously, you need the physical space in your facility for the machinery, just like with any machine.
Flatness Specs. A technical analysis and a physical leveling test should be performed to determine whether the flatness specifications on the materials can be achieved consistently.
What Are the Best Applications for Leveling?
Perforated Parts. One application for which part leveling is really needed is for perforated parts. The minute a part is perforated, it’s going to warp no matter how well the perforation is done. Perforated parts are most commonly used in the architectural industry, such as HVAC grills or architectural covers with intricate cutouts.