Addressing 8 common misconceptions about welding metal-cored wire

In some welding operations, using metal-cored wire eliminates certain nonvalue-added activities, allowing operators to spend time on other tasks that improve productivity.

Metal-cored wire is a hollow metal sheath filled with metallic powders, alloys, and arc stabilizers that provide benefits such as lower oxidation, higher impact strengths, and reduced silicon depositions in the final weld.

You might know this wire typically delivers fast travel speeds and high deposition rates, but it’s important to understand the other capabilities and limitations of metal-cored wire before using it in your arc welding operations. Let’s take a look at eight common misconceptions about this filler metal.

1. Metal-Cored Wire Is Too Expensive

Metal-cored wire, on average, costs more per pound than other types of filler metal when considering only the upfront purchase cost. However, it’s important to look at the preweld and postweld time savings, which can offset the initial cost. This can result in payback that justifies the additional investment or process change.

In some welding operations, using metal-cored wire eliminates certain nonvalue-added activities, allowing operators to spend time on other tasks that improve productivity. Since metal-cored wire tends to create little to no spatter, it eliminates the need for applying antispatter in the preweld phase or for chipping spatter after welding.

Because it also minimizes defects such as undercutting or lack of fusion, postweld activities such as grinding and rework usually aren’t necessary, saving labor time and money. Additionally, reducing postweld activities helps increase the flow of completed parts to other stages of production, such as painting or coating, improving overall productivity.

2. Metal-Cored Wire Can Weld Over Any Dirty Material

The characteristics of metal-cored wire make it especially suitable to weld through mill scale, oil, and other debris, which saves time and money in preweld cleaning. However, be aware that an excessive amount of contamination on the base metal can impede quality, so cleaning might still be required.

Most welding codes state that any excessive oil, grease, mill scale, or other debris should be removed from the weld area and adjacent area. But operations may not know what constitutes an excessive amount of contamination. If the metal-cored wire being used welds through the debris and the finished weld stays within acceptable levels for porosity, it’s fine to skip the preweld cleaning step. But when weld quality is affected, either through unacceptable porosity levels or too much weld contamination, then those contaminants should be removed in preweld cleaning.

3. Significant Deposition Rate Increases Are Always Achievable

The spec sheet for each metal-cored wire includes a range of achievable deposition rates with that wire. Much higher deposition rates are possible while still creating quality welds, and companies can sometimes achieve a 10% to 30% improvement in deposition rates, depending on how optimized their current welding process is.

But be aware that the actual deposition rate will depend on the application. Metal-cored wires are typically recommended for use with flat, horizontal welds. Using a pulsed welding process will allow metal-cored wires to be used in all positions, such as vertical-up welding, but this reduces the amperage and therefore the deposition rates that are achievable, especially compared to an all-position flux-cored product.

4. Wire Stick-Out Can Remain the Same for Metal-Cored Wire as for Solid Wire

It’s often assumed that metal-cored wire can be run with the same stick-out as solid wire, but that is not always the case. Solid wire typically requires a tighter stick-out, while metal-cored wire needs a longer one because of the wider arc and higher amount of filler metal being deposited.

When determining the proper stick-out for metal-cored wire, you need to consider three main factors: wire diameter, wire feed speed, and amperage. Typically, smaller wire diameters use a shorter stick-out. For example, with a 0.35-in.-dia. wire, a stick-out of 1/2 to 5/8 in. would be common. Using a longer one than that with a small-diameter wire will cause the wire to wander when it comes out of the contact tip. A 0.45-in.-dia. wire would use a stick-out of 3/4 to 7/8 in., while a 1/16-in.-dia. wire would use one from 3/4 to 1-1/4 in. As the wire feed speed and amperage are increased, it’s important to increase the wire stick-out. A longer one can also help improve the deposition rate slightly.

When in doubt about the proper wire stick-out, consult the wire data sheet.

5. Gun Angles Can Remain the Same for Metal-Cored Wire as for Solid Wire

When using metal-cored wire, you need to adjust the travel angle and work angle of the gun. Solid wire can often be used with either a push or a drag welding technique. But achieving a flat bead with metal-cored wire requires a 15- to 30-degree travel angle with the push technique. Using a drag technique with metal-cored wire can result in a crowned weld bead. The work angle should be 45 to 55 degrees.

If you switch to metal-cored wire in an automated weld cell, you will likely have to reprogram the gun and torch angles. Leaving those variables the same can result in faster consumable wear when using metal-cored wire. Adjusting settings such as stick-out and gun angle help compensate for the extra filler metal being added to the weld.

6. Operating Parameters Are the Same as Other Wires

The voltage and wire feed speed needed to run metal-cored wire is different than with other wires. For instance, trying to run a metal-cored wire at the same voltage and wire feed speed as a solid wire can result in undercut.